I have been using the composite oven i built to also bake the lacquer, however I cant really see any guides on the max temp we can bake lacquer to.
Im using a good quality Acrylic , the higher the temp the less long term print through i seem to get on my X-preg parts.. i've so far resisted the temptation to Bake the lacquer to 120deg c and only taken it to 85 deg c.