Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Cutting and refinishing a completed/cured sheet?
Cutting and refinishing a completed/cured sheet?
Post Reply
Like
3
Cutting and refinishing a completed/cured sheet?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Rival876
R
Rival876
posted 5 Years Ago
ANSWER
HOT
Topic Details
R
Group: Forum Members
Posts: 3,
Visits: 17
Hello all,
I need some guidance on how to modify an existing part. I have attached photos of a basic front splitter I've had laying around for some years now, and I was wonder if and how I could go about repurposing it. It is pretty flexible by my estimation so I figure if I can cut it into smaller parts, I could use it as front lip and side skirt extensions.
For the front, it would require changing the contour of the front edge to match the bumper lip, and the sides would be rectangular strips cut from the back edge of the part.
How do I go about getting clean cuts, and how should the cut edge be treated or finished? I have zero experience so I would be looking at getting tools, protection etc.
Type of front contour
Existing part
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cutting and refinishing a completed/cured sheet?
Rival876
-
5 Years Ago
The Permagrit tools. which EC sell a range of, will work well for the job you're considering The 32mm cutting disc attached to a dremel-type tool will cut very cleanly and you can improve the contro...
MarkMK
-
5 Years Ago
Hello MarkMK, Thanks for the advice. Now that you mention it I do believe I have a Dremel tool with the flex shaft extension :D Is there any need for a sealant or epoxy on that edge? Considering.....
Rival876
-
5 Years Ago
If you were really worried you could apply a thin layer of epoxy resin to the edge. Even superglue will work as a thin sealant or even brush on some lacquer carefully. You could use a rubber edging.....
Warren (Staff)
-
5 Years Ago
Thanks Warren, will give those try.
Rival876
-
5 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search