Ultimately it depends on the laminate used as well as the adhesive properties. If the part needs to be high temperature use, you might need 2 post cures, one for the part, one for the glue. Not being familiar with that specific adhesive, I do not know what its CTE or flexural strength is like so hard to say what is best. Many structural adhesives with a high flexural strength would be fine. However safer option is bond after initial post cure, then re-post cure for the adhesive if it needs it.