We are an Italian company which sells and installs natural stones, marbles.
We would like to receive a feedback from you, because our Indian marble supplier used your expoxy resin on the surface of Rainforest Green Marble with brushed finish.
We have installed this marble inside a private pool and we would like to be sure that your product doesn't affect marble under sun-light or in contact with pool water!!

Have you ever had similar experience?

Waiting for your kind reply


societàdellapietra srl
Via Cellini, 140
60019 Senigallia (AN) Italy
P.I. 02104010422
Tel. 071.7931020
wwww.societadellapietra.com
Reply
Moreno Marchetti
Moreno Marchetti
Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)
Group: Forum Members
Posts: 5, Visits: 15
Warren (Staff) - 7/8/2020 8:12:18 AM
I have no idea why they would use that resin for that application. Unfortunately there is no data and no real world experience with using VacCast in that way so I am not sure how it would last. 

Our Indian marble supplier told me that they always use your Epoxy casting resin on brushed marbles....... Sad
Which are the properties of this product for a marble?

Thanks for your availability
 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Moreno Marchetti - 5 Years Ago
Warren (Staff) - 5 Years Ago
Moreno Marchetti - 5 Years Ago
Warren (Staff) - 5 Years Ago
Moreno Marchetti - 5 Years Ago
Warren (Staff) - 5 Years Ago
Moreno Marchetti - 5 Years Ago
Moreno Marchetti - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search