Strechlon 200 bagging film


Author
Message
Big Tee Racing
Big Tee Racing
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 6, Visits: 514
Afternoon all
Can anyone point me in the direction or know where I may get hold of a small amount of strechlon bagging material ?
I have a job coming up that I don't do very often but do use the film , and I have run out 🙄

Cheers tony
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh EC are great. Super easy, and their pricing is rock solid - even for me in Aus paying the horrendous exchange rate and freight. If I was in Europe, I would get everything from them too. 
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 6/10/2020 7:55:57 AM
Yeh EC are great. Super easy, and their pricing is rock solid - even for me in Aus paying the horrendous exchange rate and freight. If I was in Europe, I would get everything from them too. 

I am surprised that there isn't a comparable supply company in the colony..... :-)

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Steve Broad - 6/10/2020 9:54:14 AM
Hanaldo - 6/10/2020 7:55:57 AM
Yeh EC are great. Super easy, and their pricing is rock solid - even for me in Aus paying the horrendous exchange rate and freight. If I was in Europe, I would get everything from them too. 

I am surprised that there isn't a comparable supply company in the colony..... :-)

There is no one supplier of everything like EC. I can piece together most things from all over the country, but it's taken a long time to build those networks.

Australia is very behind the times with composites, for the most part the industry is still pool builders and boat builders. Some of the boat builders are doing very advanced stuff, which is why these products can be sourced if you look hard enough. But it makes sense; Australia is a bloody massive place, very far away from the rest of the world, and the market is very small. I certainly wouldn't want to be in the supply game here.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Big Tee Racing - 5 Years Ago
     Try fibreglast
mporta71 - 5 Years Ago
Big Tee Racing - 5 Years Ago
             No, in the US
mporta71 - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
Big Tee Racing - 5 Years Ago
Hanaldo - 5 Years Ago
Rich (Staff) - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
                         So, no real issues, then :-)
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
explorecomposites - 5 Years Ago
BoB_from_jungle - 5 Years Ago
Hanaldo - 5 Years Ago
Rich (Staff) - 5 Years Ago
Warren (Staff) - 5 Years Ago
BoB_from_jungle - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
SleepingAwake - 5 Years Ago
Steve Broad - 5 Years Ago
SleepingAwake - 5 Years Ago
Hanaldo - 5 Years Ago
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
             Which bagging film are you using?
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago
Hanaldo - 5 Years Ago
Hanaldo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search