Group: Awaiting Activation
Posts: 3,
Visits: 13
|
Hello. I'm a relative novice at casting resin parts (from silicone molds), however I'll be needing produce quite a few parts soon, so I was thinking of purchasing a degassing chamber and vacuum pump. But I have a few questions involved in this: 1. I know about degassing silicone, but is it ok to de-gas resin that's already been poured into a mold? (to avoid bubbles in an intricate mold) 2. If question 1 is fine, would it be ok to use Easy Composites' 26L Degassing Chamber for a small piece as well? (say around the size of a golf ball) 3. Generally speaking, what is the minimum wall thickness I can produce with EC's Fast Cast Polyurethane
Many thanks to anyone who can help with any of the questions. AVA
|