Strechlon 200 bagging film


Author
Message
Big Tee Racing
Big Tee Racing
Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)
Group: Forum Members
Posts: 6, Visits: 514
Afternoon all
Can anyone point me in the direction or know where I may get hold of a small amount of strechlon bagging material ?
I have a job coming up that I don't do very often but do use the film , and I have run out 🙄

Cheers tony
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Big Tee Racing - 5/25/2020 11:41:55 AM
Afternoon all Can anyone point me in the direction or know where I may get hold of a small amount of strechlon bagging material ? I have a job coming up that I don't do very often but do use the film , and I have run out 🙄Cheers tony

Try fibreglast

Big Tee Racing
Big Tee Racing
Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)
Group: Forum Members
Posts: 6, Visits: 514
Is that in the uk ?
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Does it have to be Strechlon specifically? Easy Composites have a high elongation bagging film that is exactly the same, just a different brand.
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Big Tee Racing - 5/26/2020 9:53:52 PM
Is that in the uk ?

No, in the US

Big Tee Racing
Big Tee Racing
Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)Supreme Being (94 reputation)
Group: Forum Members
Posts: 6, Visits: 514
Hanald

I can only see two films on the easy comp site , what one are you referring to ?
Cheers tony
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!
Chris Rogers
C
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 120, Visits: 933
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Massimiliano - 5/27/2020 4:55:25 AM
Big Tee Racing - 5/26/2020 9:53:52 PM
Is that in the uk ?

No, in the US

https://www.fibreglast.com/product/stretchlon-200-bagging-film-1678/Vacuum_Bagging_Films_Peel_Ply_Tapes

Rich (Staff)
Rich (Staff)
Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)Supreme Being (2.3K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Hanaldo - 5/28/2020 12:55:00 AM
Oh, apologies, you're correct. Looks like they don't carry it anymore. Didnt notice when it got dropped!

Yes, unfortunately we haven't carried it for a couple of years now; we dropped it at about the same time as the silicone coated release ply when we moved over the the VB160 and VB200 that we stock now.

I don't know where you'd get a small amount though nowadays unfortunately.

GO