Looking for a flexible rod that wants to straighten out. Carbon fibre rods?


Looking for a flexible rod that wants to straighten out. Carbon fibre rods?
Author
Message
nigelws
n
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Noob question, sorry but there's no clear answer that I could find. 
I'm seeking a rod that is flexible enough to be wound up but which would prefer to be a straight line.
Imagine one of those auto-erecting tents that fold up into a round bag, but in this case would fold up to around 15cm diameter. Something like that would serve that purpose when piped into the outline of fabric.

I think 1, 2, or 3mm carbon rod may do for what I need but I'm not sure.

Thanks.
Edited 5 Years Ago by nigelws
Reply
nigelws
n
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Ah, shipping is a good example. Could you coil a 2mm or 3mm diameter 2000mm rod into a padded C4 (A4) envelope?