Mould for a Louver Panel


Author
Message
k.alan.bates
k
Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)
Group: Forum Members
Posts: 36, Visits: 664


I'm having a bit of a hard time conceptualizing how I would go about creating a mould for making a one-piece carbon fiber louver panel such as the one I have pictured.  

The flange around the perimeter is easy enough, but I can't quite reason how I would work out the open transition between the vane edges without making a solid transition then cutting out the opening.

Does anyone have a better idea for handling the louver vanes in a way that wouldn't require cutting out large pieces of the part during postprocess?

...has anyone made composite louvers before? What was your mold process?

Thanks everybody.
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Generally speaking, your mould would be made as a solid closed vent item.  In terms of lay up, you will need some overlap to give neat edges to trim back to. If you use pre-preg or a stabilised fabric like our ProFinish carbon cloth, you can cut the edges quite cleanly so you would only need an overlap of a mm or so to give something to sand smooth against. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
k.alan.bates
k
Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)Supreme Being (348 reputation)
Group: Forum Members
Posts: 36, Visits: 664
Warren (Staff) - 5/13/2020 11:58:30 AM
Generally speaking, your mould would be made as a solid closed vent item.  In terms of lay up, you will need some overlap to give neat edges to trim back to. If you use pre-preg or a stabilised fabric like our ProFinish carbon cloth, you can cut the edges quite cleanly so you would only need an overlap of a mm or so to give something to sand smooth against. 

So that sounds like "solid closed vent item" means "making a solid transition then cutting out the opening." 

Is my interpretation correct and does that mean my initial thought is the best way to go?

...Follow up about your use of the word 'overlap': Are you
1) referring only to the layup technique and are calling for a 1mm overlap of prepreg material

or

2) are you referring to a ~1mm return molded into the louver vents to allow the trim to marry up with the backside of the vanes rather than the leading edge?

Thank you very much for your assistance.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
k.alan.bates - 5 Years Ago
Warren (Staff) - 5 Years Ago
k.alan.bates - 5 Years Ago
Warren (Staff) - 5 Years Ago
beliblisk - 5 Years Ago
     My vent mould .
Steve Broad - 5 Years Ago
Hanaldo - 5 Years Ago
Warren (Staff) - 5 Years Ago
k.alan.bates - 3 Years Ago
Warren (Staff) - 3 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search