Would I be better with Prepreg ?


Author
Message
Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Chris Rogers - 5/5/2020 9:16:03 PM


Here's a video of the wet-preg method - not super helpful for a flat panel - but it's just to show the process:  https://youtu.be/06-0Vxs_9nY  

Hi, the link is not working... could you please repost it?
Thanks

Damien
Damien
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 32, Visits: 132
Now except for paying attention when putting the release film as flat as possible, any other tip to limit the little
"folds" of resin on the part that is not against the mould ?


Thanks !
Chris Rogers
C
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 120, Visits: 933
Massimiliano - 5/10/2020 4:25:52 AM
Chris Rogers - 5/5/2020 9:16:03 PM


Here's a video of the wet-preg method - not super helpful for a flat panel - but it's just to show the process:  https://youtu.be/06-0Vxs_9nY  

Hi, the link is not working... could you please repost it?
Thanks

Sorry - fixed it in the original post.  





Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Chris Rogers - 5/11/2020 1:20:43 AM
Massimiliano - 5/10/2020 4:25:52 AM
Chris Rogers - 5/5/2020 9:16:03 PM


Here's a video of the wet-preg method - not super helpful for a flat panel - but it's just to show the process:  https://youtu.be/06-0Vxs_9nY  

Hi, the link is not working... could you please repost it?
Thanks

Sorry - fixed it in the original post.  

Thank you!