Hi, I wonder if you can give me some advice on fixings for carbon fibre strips.

I'm woking on a project at the moment which requires me to provide a hole in one end of a cbrbon fibre strip to act as a 'fixed' fixing point for a screw to go through and a slot at the other end to allow for movement in the finished article as it needs to retain a degree of flexibility in use. I'm undecided about width and thickness of the strip I will need but would appreciate some advice if there is a minimum you would not recommend going below to avoid the risk of cracking or splitting whilst drilling the hole.

For the slotted end would a router be suitable for cutting the slot out of the material? Also, I am new to using carbon fibre and wondder if there are any perticular health and safety issues in cutting the material - i would be using a mask and protective glasses as a matter of course, but would I need to consider anything other than that?

As an alternative, I am also thinking about possibly using a solid rod of small diameter as this would make some other design issues easier to deal with, but I am a bit stuck when it comes to figuring out how this might be fixed - is there any sort of end connector (see attached rough sketch) available which could be fixed to the end of a rod to allow it to be screw-fixed in place?

I'd be grateful for any guidance you might be able to give
Attachments
end fixing sketch.pdf (377 views, 96.00 KB)
Reply
davidg
davidg
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 2, Visits: 16
many thanks for your advice - very helpful