How to extend polyester resin pot life?


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hello,
what are the ways to extend the pot life of polyester resin (if possible)?

Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
I never had any problems. It worked just as intended with about 15 different polyester resins. Never tried it with vinyl, because I only have the two vinyl components of the unimould system and those aren't that fast anyways.
Maybe I should be careful in the future.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
mporta71 - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search