I would like to degass the AS40 silicone.  it is the first time I use this Easycomp material.  

 I am using a VE115SV 1/4HP pump.  It seems that the silicone isn't degassing completely. 

could it be that the pump has to less power to degass?  the silicone starts to bublle, but doesn't make the self collapse. 

pix of a sample i made

and the finished result



Replies
dubster
dubster
Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)
Group: Forum Members
Posts: 15, Visits: 126
It now makes the selve collapse, but it takes ages to degass it completely.  

in this times where materials aren't easy to receive, Is it a shame to use a first silicone (that degasses much faster) for casting on the visual side, let it cure and then use a second one 'to fill the space'?

both silicones have the same shore value...
Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
dubster - 4/20/2020 9:27:56 AM
It now makes the selve collapse, but it takes ages to degass it completely.  

in this times where materials aren't easy to receive, Is it a shame to use a first silicone (that degasses much faster) for casting on the visual side, let it cure and then use a second one 'to fill the space'?

both silicones have the same shore value...

Shouldn't be an issue if you get the timing right and pour the second batch of silicone when the first pour is still tacky. But this will always be a touch weaker than a single pour. Depends how many times you want to use the mould as to whether that will matter or not.


dubster
dubster
Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)Supreme Being (235 reputation)
Group: Forum Members
Posts: 15, Visits: 126
Hanaldo - 4/21/2020 5:51:45 AM
dubster - 4/20/2020 9:27:56 AM
It now makes the selve collapse, but it takes ages to degass it completely.  

in this times where materials aren't easy to receive, Is it a shame to use a first silicone (that degasses much faster) for casting on the visual side, let it cure and then use a second one 'to fill the space'?

both silicones have the same shore value...

Shouldn't be an issue if you get the timing right and pour the second batch of silicone when the first pour is still tacky. But this will always be a touch weaker than a single pour. Depends how many times you want to use the mould as to whether that will matter or not.


Thanks for the advice!! 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search