As said, it might be cheaper an easier to sell on the lightweight boat and get something more heavy duty.
However, if that is not possible, it is possible to add extra reinforcement to the hull. You would need to sand back to the fabric, and wet lay on additional layers of fabric to get the desired additional strength. Then finish it off with a layer of resin, sanded smooth then polished, to give the nice level finish to the out side of the hull.