Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I wouldnt bother sanding it, it typically doesnt work well and theres a chance you hit your mould which would be bad. Just layup a layer or two of 225g CSM with polyester or vinyl ester resin onto it and use that to pull it off the mould cleanly. Your mould should be fine, but the gelcoat is wasted. Better to waste it with a few more cheap materials rather than expensive ones.
|