Glue for carbon to PP plastic


Author
Message
Carbonman
Carbonman
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 18
Hi, I made some cf parts and want to glue a frame of PP plastic to the back. The back is peel play foil so will have a good stick to it. Not sure about the glue I need to bount the parts. CA? Or the epoxy from EAsyComp?
Hope you can help
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
In an older topic, I think Matt from EC said that he would use Structural polyurethane adhesive for composite to composite bonding.

Also said he would use epoxy to bond composite to metals.

Hope it helped.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Dave
Dave
Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)Supreme Being (478 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Use a structural adhesive you will have to check about compatibility of types of resins like epoxy, polyester, acrylic. The texture left by the peel ply will leave a reasonably good bond surface.

 However many people suggest you will get a better bond if you sand the surface with some coarse grit, maybe 80 or 120grit or something like that. If you do this be very careful to not sand down to the fibres, only enough to roughen the whole surface. Also make sure you clean the bonding surface with a de greaser before and after you sand it - this can make a huge difference, degrease even if you just use the peel ply surface.

Dave.
Edited 13 Years Ago by Dave