Ok guys, I have all the materials, I have the moulds so what do I do now?

Can anyone tell me what goes first and how long do I wait before the next step.

I have:

Easy-Lease release agent

#8 mould release wax

GC50 Gelcoat (Do I need to spray this on)

And

Epxoxy and hardner (fast and slow)

I am confused as to what order the first 3 go and are they all needed?

Part is a hand lay Kevlar roof vent.

Is there any beginner guide for dummies I can read through.
Reply
Kevin-Lee
Kevin-Lee
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 44, Visits: 2.4K
Hi,

This will answer all your questions.

Note the first 2 videos on the page, should get you in the right direction...

Kev.
Edited 13 Years Ago by Kevin-Lee
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search