I've been skinning quite a few parts with the XCR process and working out various issues along the way.

I have built a post-cure oven (insulated MDF enclosure) - however, I inadvertently left a part under a halogen lamp on my worktop (I use the lamp for inspection and some localized heat for lay-up) and noticed that after maybe 20-30 mins the epoxy had 'sunk' into the carbon and given me a degree of print through.

Now - initially a bit of a mistake, however it got me thinking.

When skinning components where mechanical properties are not as vital as the final finish and ensuring print-through doesn't happen in service (car interior trims), could I use this high heat - short term technique to vastly reduce my post-cure times - and thus part turnover time?

Is this something worth looking into further, or am I committing a cardinal sin by not running through a full 16 hour post cure process? (as above - this is skinning so mechanical properties are irrelevant in comparison to ensuring print through issues don't arise when the parts are sat in a hot car on a summer's day)

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The problem is the cosmetic finish will suffer from the sinking. However if the resin was thick enough to sand that out then the cosmetic issue wouldn't be a problem.  The mechanical properties may suffer slightly as will HDT from the rapid curing but for most automotive applications you aren't always pushing the limits anyway,

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search