Xencast px90 too flexible on a thin part
Xencast px90 too flexible on a thin part
Post Reply
Like
3
Xencast px90 too flexible on a thin part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
8900120d
8900120d
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 939
I’ve made a silicone mould of a thin part (roughly 1mm thickness 100mm long)
Mixed the px90 at 1:1 ratio, and poured it into the mould.
3hours later I went to demould it and it’s super flexible (I can scrunch it up like paper) and I can rip it !
Isn’t the px90 supposed to be hard ? Is my part too thin to use px90?
Thanks
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Shore hardness and flexibility are 2 different properties. Although often related in materials - ie often a hard material is also rigid, this is not always the case.
You may in this case be better off looking at a rigid PU resin? If you want it quite tough (some fast cast resins are brittle in thin sections.) then look at something like our
Xencast P6 Toughened Polyurethane Casting Resin
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
5
8900120d
8900120d
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 37,
Visits: 939
Thanks a lot for your response
would the xencast p6 be flexible enough to take light impact without snapping?
Reply
Like
5
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Being a toughened PU resin, it is likely to be ok depending on severity of impact, thickness cast etc. It is certainly a lot tougher than your typical PU casting resins.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search