Additional stiffening would help but care needs to be taken not to make it worse. You can wrap it in release film or similar and use an electric blanket to get a mild post cure which should help. The release film will stop the blanket sticking.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|