Mould reinforcement when?


Author
Message
Classicarbon
C
Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)Supreme Being (768 reputation)
Group: Forum Members
Posts: 86, Visits: 639
Just got mould drying up.I want make reinforcemen.Do it before taking out original part or after?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Ideally add any mould reinforcement at the same time as initial moulding.  That way you reduce the chance of any warping or distortion of the mould as the pattern is still in it to stabilise the shape. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO