Hi All

New to this forum and in need of a little help, part of my mould has alot of spider cracks and part of the gel has come away from the mould, whats the best way to repair this they are on a curved section of the mould. Advice would be much appricated

Callum
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
hi,

I had the same problem a few times, due to a to cold environment and resin not mixed well enough Blush, my bad.
What I did was start again; Because I didn't know what caused the problems and wanted to find out what the problem was.
It was a small part 25x25cm. 

- I don't know how big your part is but you could sand it of, back to the fiber (don't go to deep!) and put some resin on it (few layers with sanding inbetween the layers)
- Or if you have Gelcoat chipping of you maybe remove it with a hammer and chisel, but you'l have to be very carful not to go into the fiber.

just like you can read those are timeconsuming steps... and its sometimes easier to start again.

Maybe a picture of the part could help to give more/other advice.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search