Hi, I took delivery of a 250ml bottle of the board sealer last week. Bearing in mind the sensitivity of this fluid too moisture, is it normal for the container not to have a secondary seal underneath the screw cap? Best Regards  Ian Gough


Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The seal is against the lid and the edge of the bottle top.  The seal is good enough that a secondary tamper seal is not needed inside the bottle.  All bottles are also nitrogen purged to aid reducing degradation during storage and transit.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Ian.gough
Ian.gough
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 2, Visits: 12
Warren (Staff) - 11/4/2019 5:19:50 PM
The seal is against the lid and the edge of the bottle top.  The seal is good enough that a secondary tamper seal is not needed inside the bottle.  All bottles are also nitrogen purged to aid reducing degradation during storage and transit.

Thanks for your reply Warren. Just not what I was expecting when most (all?) release agents etc. have that secondary seal!