Hi boys!

My oven doesn't work jet and I put my new mould outside of the workshop. 4 pieces split-mould dissasembled and been put separately in the sunlight. Gelcoat side face to the sky. Surface reached 50-55 degree Celsius for a couple hours. When I was putting the parts together just noticed that the front panel is not fitting perfectly. Cause of the distorsion of the side panels. Can I solve this somehow? Let's say with controlled post cureing (with assembled mould)?
With some force I can push back the sides in position so still can use the mould. Just annoying...
Vinyl gelcoat, 2x100gm2 CSM coupling coat, 4x450gm2 CSM with tooling resin.
Pictures attached. Distorsion is about 10-12mm.
Any idea why this happend?

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh the sun is a really uncontrolled method of heating, and composites require really precise control. Not only is the ramp rate way too fast as KL mentioned, but there's also a good chance you got uneven areas of heat where some parts of the mould may have cast a shadow on themselves. If this happens, you have some parts of your mould getting up to 50°, and other parts still sitting at 20° or whatever. This is a disaster and will easily warp parts.

There is a good chance you can restore the mould however, but you will likely need your oven running well. If you bolt the parts together in proper position and then cure them above your previous temperature (I would do 70-80°), they will likely hold that position and fit back together well again.