+x Legoman - 9/17/2019 8:02:00 PMAs you can see there are different colours on the cured mould surface. Probably I failed with lamination and got some air under the last layer...any idea?
+x noahark - 9/17/2019 10:20:39 PM+x Legoman - 9/17/2019 8:02:00 PMAs you can see there are different colours on the cured mould surface. Probably I failed with lamination and got some air under the last layer...any idea?What tool & resin did you use to wet it out? Any heat applied in the process? What type of fiberglass mat was used? What ambient temperature did it cure at? Does it really matter if the other side is clean?