Hi All,

I've just joined the forum as this place seems to contain a wealth of knowledge and I'm looking for some help!

I'm trying to cast some large resin plinths. They'll be up to 50cm cubed and will be hollow but with walls about 20-30mm thick.

I'm basically trying to recreate this effect in the image below which are polyester resin. However, from researching polyester resin it seems that I'm going to have problems with shrinkage/warpage and dealing with overheating. Some people have advised me to use epoxy but obviously it's a lot more expensive.

Can anyone shed any light on how the below have been made with polyester resin?

Thanks



Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Filler powders can certainly help thermal stability and reduce shrinkage so yes it might help.  Just be careful how much you use as most, in significant quantity, will turn the casting white, so you may need to take this into account.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search