Hi all,

I am new to composites and I am currently trying to skin some parts for my car.

To begin, I had issues with bonding the fabric to the parts but I have seemed to solved my issue by not folding the excess behind the part for a clean edge. My main issue at the moment is sanding. I am struggling to get a nice flat surface and I am reluctant to use 120 to begin flatting as I always end up with scratches I struggle to sand out. What is the most efficient way to get a smooth finish without sanding forever. Also, what is the best way to remove drips that have cured and also a bulging edge where the resin has collected on a vertical edge on a part? I worry when I’m sanding I will hit the fabric.

My last issue seemed to be on the weave when I finished sanding, it looks like a void between the resin and the weave as well as moisture under the resin when damp outside.

I am using XCR resin and have been told it is self levelling and does not have air bubbles but I keep getting bubbles!

Thank you


Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You should always take care when sanding at 120 grit as you do take off a fair bit of material.  There is no harm in taking off the high spots to level it out, keying the rest at 120, then re-coating to avoid going through the fabric. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
If a better gloss finish is desired also, it's worth going up to 1500 grit, at least, as 1200 grit can take quite a bit of machine polish work to get to a good shine, especially with a relatively hard epoxy. 

If I'm doing any repair jobs using epoxy, I usually go up to 2000 grit, which usually results in only needing a couple of passes with the polisher to get a good gloss. If you're parts are large, though, this might feel a bit too laborious, but going to 1500 will likely make getting a good shine a lot easier


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
LukeSGee - 6 Years Ago
MarkMK - 6 Years Ago
Warren (Staff) - 6 Years Ago
LukeSGee - 6 Years Ago
MarkMK - 6 Years Ago
Warren (Staff) - 6 Years Ago
LukeSGee - 6 Years Ago
Warren (Staff) - 6 Years Ago
MarkMK - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search