Using the infusion mesh and peel ply in tight areas


Author
Message
Carbon Tuner
Carbon Tuner
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 104, Visits: 422


Howdy.



WellI am trying to make a rather small part. It is the knuckle cover for a seatbelthinge. 9x7 cm and bout’ 3 cm deep, in the shape of a triangle.



What’sthe correct way to get that mesh and peel ply to go in all the tight areas? Ihave been cutting the peel ply in strips and over lapping it, and the mesh Imake it in to parts, then snip the edges so the flex better..



Thanksfor any help!



Donnie





If Brute Force Isn''''t working your not using enough...
Replies
NikCFC
NikCFC
Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)Supreme Being (557 reputation)
Group: Forum Members
Posts: 61, Visits: 871
I haven't used the ElastiFilm from Easy Composites but I know that when doing infusion you shouldn't use elastic fil because it clogs the flow mesh's pores and as a result the air and resin move very slow. I would like to get an opinion from EC crew though.
fgayford
fgayford
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Here in Canada the name is Stretchelon. It infuses just fine over any flow media I have tried. I have never heard of someone saying it restricks flow.

Fred 