			            Silicone moulds can't be used for making carbon parts, at least not ones with any degree of accuracy required. Composite parts need rigid moulds.
  You could do the mounting clips with silicone moulds, and potentially the storage and cup holder areas as well. If you made silicone moulds of these parts and then cast them with a rigid polyurethane, you could then bond them to the completed carbon surround.
  This sort of thing does need to be redesigned somewhat, you can't make it in the same way as OEM.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |