+x ljac133 - 4/20/2018 12:47:46 PMHi,New to composites and would like some adviceI'm looking to achieve something similar to Adam Hansen's 'Hanseeno' cycling shoes - here's a video with him talking about them: https://cyclingtips.com/2014/05/adam-hansens-custom-shoes/I've ordered a started kit and some unidirectional sheets from easycomposites and I've got a vague idea where to start.I'm most worried about keeping the uppers flexible enough (Hansen talks about using a different resin there for this reason), and joining different parts to make a whole if I construct the shoes in sections.ThanksLuke