Lay visqueen on your table. Put your cloth on it. Wet out the cloth the best you can. Then add another layer of visqueen on top. Use a squeegee on top of the visqueen to move the resin to areas that are dry. Boat builders use this method all the time.
This also makes transferring the cloth to you mold much easier. Just peel the top layer I’ve visqueen off and move it over to your mold using the bottom layer.
Jason
|