Group: Forum Members
Posts: 18,
Visits: 54
|
This is from your website:- GlassCast 10 is formulated as a casting resin, not a coating resin. This means that whilst it offers the advantage of incredible clarity - even in thick sections - it does not cure with a perfect surface on the open face in the way that our GlassCast 3 coating resin does.
What does that mean its not a perfect surface?
|