Group: Forum Members
Posts: 5,
Visits: 367
|
Guys
I am after some advice please.
I've done a bit of wet layup and vacuum bag CF composite ( only simple stuff ! ) but am now looking to use infusion to create a flat panel ( approx 400mm x 900mm ) between two pieces of glass ( to be used as wing end plates on a hill climb car ). The construction would be :-
Gel coat-CF-Soric-CF-Gel coat
My question is, the two pieces of glass ( top and bottom mould ) will be larger than the composite stack so how do you stop the resin taking the "easy route " around the composite stack and not wetting out the CF etc fully ? ( assuming the resin input is one end and the vacuum the other ).
Thanks in advance.
Adrian
|