Group: Forum Members
Posts: 550,
Visits: 27K
|
Yes and no. Grams No, ml yes. If you mix by weight it's still 100/45 or a multiple/fraction of that. You could use 20/9 by weight (No syringes, only a cup on a scale), wich would be close to your desired 24g. Syringes will give you a certain volume, therefore it's 2:1 By weight= 100:45 by volume= 2:1 Always.
|