Wpreg 110 or 130 for pressmolding?


Author
Message
Kalle Ström
Kalle Ström
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 1, Visits: 9
Going to make some 4mm thick kind of complicated carbon pieces using the eb700 and press together to get nice surface on both sides. Wich prepreg is best suited for this? X110 or x130?

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If you are using the EB700 epoxy tooling block then I would stick with the XC110.  The XC130 is designed for autoclave use or press use with similar pressures.  The EB700 tooling block is not designed for use under such high pressure uses.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search