Correct Resins/Materials for Pulling Carbon Parts?


Author
Message
drxlcarfreak
d
Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)
Group: Forum Members
Posts: 7, Visits: 170
I am getting ready to embark on my first carbon fiber part and want to make sure that I have the correct materials/process down. I am planning to CNC cut extruded polystyrene to make base plugs from, which I plan to under cut and coat with a layer of fiberglass and then body filler to then do the final machine pass on so that I have a hard dimensionally accurate surface I can then final sand and polish. I plan to use epoxy resin so the foam won’t melt on me. For the mold, I plan to use polyester resin so that I can use CSM for tighter contours, easier wetting out and to reduce overall costs. For the carbon fiber parts, I plan to use an epoxy compatible poly/vinylester clear top/gel coat and use infusion resin for the carbon fiber layers.

Plug:
-    Lowes/Home Depot XPS Foam
-    Fiberglass Cloth layer – US Composites 635 thin resin with fast hardener – Is this layer needed or will the fair compound alone be rigid enough to pull a mold from?
-    Body filler layer – US Composites 635 thin resin with fast hardener and US Composites Fairing Compound

Mold:
-    Plug Sealer – McLube 1038 Sealant and release agent
-    Plug Release – McLube 1123 High-Gloss Release agent
-    Gel Coat – US Composites Orange Tooling Gelcoat 
-    CSM Layers – US Composites 404 Tooling Polyester Resin

Part:
-    Mold Sealer – McLube 1038 Sealant and release agent
-    Mold Release – McLube 1123 High-Gloss Release agent
-    Gel/Clear Coat – Duratec 904-061
-    Carbon Fiber Infusion Epoxy – Pro-Set INF-114 and INF-211 hardener

I have researched quite a bit and without just buying one of everything and testing it out, this SEEMS like the best/cheapest way forward. I obviously also need to get the fiber glass and carbon fiber sheets as well as the materials for the infusion process, but the resins and release agent compatibility is what has got my head spinning at the moment. I know I like the idea of the Duratec clearcoat as an added buffer layer between the polyester mold and the epoxy part as I have read issues where epoxy can bond to the polyester through the release agent coats sometimes, but there may be a better/cheaper option. I know this is less “science” and more an artform on what materials are best together, but does anyone have any suggestions on better/different/cheaper/faster/whatever materials? Are there any compatibility issues with anything?

Thanks guys!

Replies
drxlcarfreak
d
Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)
Group: Forum Members
Posts: 7, Visits: 170

Did I post this in the wrong section or something? Does anyone have any input?

Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
drxlcarfreak - 3/8/2019 5:15:16 PM

Did I post this in the wrong section or something? Does anyone have any input?

It's just a very long post and chances are noone here used all of the above materials. I certainly did not use any of them, but your approach seems reasonable and you are asking the right questions in terms of compatability.

I would call the shop and ask. And then make a small part to test everything!

Let us know how things are working out

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search