I have found one on-line vendor offering  UV inhibitor, but the video tutorials that are available do not discuss the need for any added step to protect carbon fiber products. Will the resin used in all three methods of Carbon Fiber fabrication (Resin Infusion, Hand Layup, and Prepreg) have UV inhibitors included in the resin chemistry?


A Lifelong Learner

Reply
John Hansen
J
Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)Supreme Being (379 reputation)
Group: Forum Members
Posts: 42, Visits: 232
Lester Populaire - 2/14/2019 8:14:17 AM
HansenJC - 2/13/2019 6:57:54 PM
I have found one on-line vendor offering  UV inhibitor, but the video tutorials that are available do not discuss the need for any added step to protect carbon fiber products. Will the resin used in all three methods of Carbon Fiber fabrication (Resin Infusion, Hand Layup, and Prepreg) have UV inhibitors included in the resin chemistry?

they usually do not. if you want serious UV protection i would recommend an automotive clearcoat on top of your parts.


Thank you. My UAV parts will get rare and short exposure to sun.


A Lifelong Learner

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search