Group: Forum Members
Posts: 2,
Visits: 4
|
Hi I am having problems with bubbles in my Xencast P6 castings. I read through the forum for answers first, and can confirm that the temperature and humidity would seem normal, as I am doing the casting in the home. The product I have is now 2 years old, and when first used I would have the occasional bubble in the casting, which I would expect, however the last few casting are literally covered in bubbles looking almost like an "Aero" chocolate bar. Though I cannot see a "best by" date on the product, I was wondering if the issue is age, many thanks for your assistance.
|