+x smee - 2/2/2019 1:04:50 PMYou are advertising Translucent Tinting Pigments, Pack of 6 for £8.45 plus VAT. Are these mixable pigments suitable for use with Xencast P2 Polyurethane Casting Resin. I am happy to experiment to obtain any depth of colour as long as I know that these pigments are compatible with P2. Thanks
+x Matthieu Libeert - 2/6/2019 7:09:46 PM+x smee - 2/2/2019 1:04:50 PMYou are advertising Translucent Tinting Pigments, Pack of 6 for £8.45 plus VAT. Are these mixable pigments suitable for use with Xencast P2 Polyurethane Casting Resin. I am happy to experiment to obtain any depth of colour as long as I know that these pigments are compatible with P2. Thanksto add to what warren is saying; if you add enough pigment it will work but the base colour is white so keep in mind that if you don't add enough red for example you'll end up with a pink part if you'r looking for translucent coloured parts you'r better of with the glasscast products...only downside is longer curing