That could be done by pretty much any method. I would probably get some aluminium sheet and fold it into that shape to give you a mould which you can infuse the sheet. If your carbon layup gives the same thickness as the aluminium then it should be just as stiff if not stiffer while being significantly lighter.. You could also do some cut outs to save weight if needs be.