Hi everybody,

How do you restore a full gloss finish on EG160 after making some repairs? Searching for best practice 😉
Reply
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
NW1 for sure but I would avoid EasyGloss because of the Wax content; if you had it, you could finsih with some of the TopFinish2.