Hi everybody,

How do you restore a full gloss finish on EG160 after making some repairs? Searching for best practice 😉
Replies
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
EG160 isn't too bad to polish, you need to work through finer grits of wet/dry abrasive papers up to around 1500grit before switching to a suitable polishing compound and you should restore the gloss to a level similar to that of the rest of the mould surface.
SHaas
S
Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)
Group: Forum Members
Posts: 46, Visits: 383
What is a suitable poslihing compound? Usually I you the ones from EC... easygloss and nw1.