Glasscast 50 polishing options


Author
Message
Chris M
Chris M
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Hi, I need some help with polishing options please!

I have made a river resin table using glasscast 50. I used a metallic tinting pigment, it looked a lot more opaque in the bucket than in the final outcome which is mostly transulscent.

Having sanded (currently at 120 grit) I prefer the matte and opaque finish - partly because its truer to the colour I was after originally, but also because I made a few mistakes in the resin which thankfully disappeared under the cloudy effect after sanding.

What polishing options exist which will get a transulscent glasscast 50 to polish up to a cloudy sort of matte finish that will mask any minor problems in the resin eg I tried to drill out a dust spec and fill with an attempted colour match which didnt work at all Sad

N.B I’m planning on using a clear osmo topoil on the wood.

Any help much appreciated

Thanks

Chris


Replies
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Chris Mawer - 12/27/2018 8:58:59 PM
Hi, I need some help with polishing options please!

I have made a river resin table using glasscast 50. I used a metallic tinting pigment, it looked a lot more opaque in the bucket than in the final outcome which is mostly transulscent.

Having sanded (currently at 120 grit) I prefer the matte and opaque finish - partly because its truer to the colour I was after originally, but also because I made a few mistakes in the resin which thankfully disappeared under the cloudy effect after sanding.

What polishing options exist which will get a transulscent glasscast 50 to polish up to a cloudy sort of matte finish that will mask any minor problems in the resin eg I tried to drill out a dust spec and fill with an attempted colour match which didnt work at all Sad

N.B I’m planning on using a clear osmo topoil on the wood.

Any help much appreciated

Thanks

Chris


Sand till a higher grit without polishing will result in an opaque finish... start with 120 like you did, go up till 200 - 400 - 800 - 1000. 
1000 grit should leave you an opaque finish, if you want it less opaque go higher in grit, if 1000 is to glossy go back down in grit


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Chris M
Chris M
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 9
Thank you very much, that is great news!