Group: Forum Members
Posts: 237,
Visits: 4.8K
|
To be fair not that much more. Put a vernier on a piece of uncurred umaterial an that's the thickness you will get cured,be it 15psi or 90 Just loose a little bit on a ply stack with multiple layers as one layer fits into another Don't really need 90psi,but your 100% it's in the corners Even 30psi will give you 99% success
|