After infusing in a multi-part mould, very thin layers of cured resin remain at the interfaces between the mouldings. This resin is very difficult to remove, and if there is just a little bit of it left, the parting surfaces will not work properly together. The gap between the mouldings is then getting bigger with every infusion. It takes me almost a full day to cleanse the interfaces. So far I have treated the parting surfaces between the mouldings with AFH-1 (wax mixture in solvents). With which release agent do I best separate the flange surfaces between the moulded parts? And can a mould cleaner help?