I would like to cast a pin badge in to the handle of a walking stick which is Lignum Vitae wood. Can you please advise me the correct resin to select?
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It depends on the exact thickness but from what I have seen, most stick handles are reasonably chunky to afford a good grip, so I would go for the GlassCast 50 Clear Epoxy Casting Resin


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search