Flat sheet


Author
Message
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
I'm looking to make some flat sheets about 1000x1000mm is ther3 anything other than glass I can use to keep the sheet flat as I'm struggling to find a sheet of glass that size at a reasonable price. 
Can I use thick perspex and lay it on that? 
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Polypropylene sheet is your friend in cases like this.  Off the shelf it usually has a high gloss finish and naturally does not stick to any resin systems.   If it is cosmetic sheet, try and get one with backing plastic as the sheet can scratch in transit and handling.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search