I have a carbon bike frame which I am trying to strip the paint off to respray.
I have tried solvent free paint strippers but they won't break down the clear lacquer despite leaving for 24 hours wrapped in cling film.
Does anyone know of a paint stripper which is kind to carbon fibre but can remove paint?