Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi, as the guys have suggested curing at a lower temperature for longer is not a great substitute for curing at or closer to the recommended 20'C. If you're looking at more like 15'C then you would be OK to just let it cure for longer but anything much less than that and you would start to see cured properties that are not what they would have been if the part had been cured at a more appropriate temperature. A rule of thumb for how temperature affects time is to double (or halve) values for every 10 degrees C increase or decrease. This means that at 10'C the resin would have twice the pot life and take twice as long to cure as it would at 20'C. At 30'C you would have half the pot life and it would cure in half the time. I wouldn't suggest using this rule to go much below the recommended cure but it's very handy when you're working in ambient temperatures above the quoted 20'C.
As Oakmont points out, the viscosity and handling of the resin will also be quite different and is likely to cause problems at lower temperatures and you should be aware that the lower the cure temperature, the lower the Tg (effectively the temperature tolerance) of the cured resin.
So, with all this said, it's definitely best to try to do your work in an environment as close as you can get to 20'C. We all know that this isn't always possible and you will still find that the resin cures (albeit slower) at 15'C or even 10'C but you will be compromising the mechanical properties and the behaviour of the resin if you stray too far from optimal conditions.
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|