Ideally stick with 2 pack fillers if you use them. A lot of people have problems with 1 pack fillers, primers and paints on the pattern causing a sticker in the mould as they can outgas especially when recently sprayed.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|